Bøker Bok 110 av 14... into the globe intended to be silvered; the alloy should be poured into the globe...
" ... into the globe intended to be silvered; the alloy should be poured into the globe by means of a paper or glass funnel reaching almost to the bottom of the globe, to prevent... "
The Emporium of Arts & Sciences - Side 365
redigert av - 1814
Uten tilgangsbegrensning - Om denne boken

The Cabinet of Arts: Or, General Instructor in Arts, Science, Trade ...

Hewson Clarke, John Dougall - 1817 - 859 sider
...fire, and before it grows eold, add five ounces of mercury, and stir the is hole well tc^i-ilier ; thru put the fluid amalgam into a clean glass, and it is fit for use. When this amalgam is iiM-d ('. u- fpiUug or severing, let it first be strained through a linen, mg ; tjhpn, gently pour...
Uten tilgangsbegrensning - Om denne boken

Elements of Science and Art: Being a Familiar Introduction to ..., Volum 2

John Imison - 1822
...venture to take it up, But before you take the weights off, gently brush the edges of the glass, that no mercury may adhere to them ; then take it up, and...through a linen rag ; then gently pour some ounces of it into the globe intended to be foiled : the mixture should be poured into the globe, by means...
Uten tilgangsbegrensning - Om denne boken

Elements of science and art: being a familiar introduction to ..., Volum 2

John Imison - 1822
...for if, when taken up, it is immediately set perpendicular, air will get in between the foil and tin- glass at the top, as the mercury descends to the bottom...amalgam into a clean glass, and it is fit for use. When tlu's amalgam is used for foiling or silvering, let it first be strained through a linen rag ; then...
Uten tilgangsbegrensning - Om denne boken

The Gilder's Manual: A Complete Practical Guide to Gilding in All Its ...

1876 - 135 sider
...caref ally skim off the dross ; remove the alloy from the fire, and before it grows cold add 5 oz. of mercury, and stir the whole well together ; then...and it is fit for use. When this amalgam is used for silvering, let iv be first strained through a linen rag ; then gently pour some ounces thereof into...
Uten tilgangsbegrensning - Om denne boken

Workshop Receipts: For the Use of Manufacturers, Mechanics and Scientific ...

Ernest Spon - 1879 - 450 sider
...and carefully skim off the dross ; remove the alloy from the fire, and before it grows cold add 5 oz. of mercury, and stir the whole well together ; then...and it is fit for use. When this amalgam is used for silvering, let it be first strained through a linen rag; then gently pour some ounces thereof into...
Uten tilgangsbegrensning - Om denne boken

Workshop Receipts ...

1883
...and carefully skim off the dross ; remove the alloy from the fire, and before it grows cold add 5 oz. of mercury, and stir the whole well together ; then...and it is fit for use. When this amalgam is used for silvering, let it be first strained through a linen rag; then gently pour some ounces thereof into...
Uten tilgangsbegrensning - Om denne boken

American library edition of workshop receipts: being a complete ..., Volum 1

Ernest Spon - 1903
...alloy from the fire, and before it grows cold add 5 oz. mercury, and stir the whole well together l then put the fluid amalgam into a clean glass, and it is fit for use. When this amalgam is used for silvering, let it be first strained through a linen rag ; then gently pour some ounces thereof into...
Uten tilgangsbegrensning - Om denne boken

Workshop Receipts ...

1906
...from the fire, and before it grows cold add 5 oz. mercury, and stir the whole well together ; then pat the fluid amalgam into a clean glass, and it is fit for use. When this amalgam is used for silvering, let it be first strained through a linen rag ; then gently pour some ounces thereof into...
Uten tilgangsbegrensning - Om denne boken

Henleys' Twentieth Century Book of Recipes, Formulas and Processes ...

Gardner Dexter Hiscox - 1907 - 781 sider
...bismuth, and carefully skim off the dross; remove the alloy from the fire and before it grows cold add 5 ounces of mercury, and stir the whole well together;...amalgam into a clean glass, and it is fit for use. AYhen this amalgam is used for silvering 642 1ft it be first strained through a linen rag; then gently...
Uten tilgangsbegrensning - Om denne boken

Workshop Receipts, for Manufacturers and Scientific Amateurs: Joint pipes

1909
...and carefully skim off the dross ; remove the alloy from the fire, and before it grows cold add 5 oz. mercury, and stir the whole well together; then put...and it is fit for use. When this amalgam is used for silvering, let it be first strained through a linen rag ; then gently pour some ounces thereof into...
Uten tilgangsbegrensning - Om denne boken